MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Elmet Technologies

Elastocon TPE Technologies Elastocon® 8058BL Thermoplastic Elastomer  (discontinued **)
Categories: Polymer; Thermoplastic; Elastomer, TPE

Material Notes: Elastocon® 8058BL is a black lubricated thermoplastic elastomer formulated for applications that require rubber-like properties and a reduced coefficient of friction. Elastocon® 8058BL is well suited for consumer goods and industrial applications requiring U.V. stability. Elastocon® 8058BL can be overmolded to polypropylene.

Information provided by Elastocon TPE Technologies, Inc. Elastocon® TPE Technologies has been acquired by Aurora Plastics.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 1.04 g/cc1.04 g/ccASTM D792
Linear Mold Shrinkage, Flow 0.012 - 0.022 cm/cm0.012 - 0.022 in/in
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore A 6060ASTM D2240
Tensile Strength, Yield 6.69 MPa970 psiASTM D412
Elongation at Break 702 %702 %ASTM D412
100% Modulus 2.39 MPa
@Strain 100 %
347 psi
@Strain 100 %
ASTM D412
Compression Set 17 %
@Time 79200 sec
17 %
@Time 22.0 hour
ASTM D395B
 
Processing PropertiesMetricEnglishComments
Feed Temperature 79.0 °C174 °F
Rear Barrel Temperature 174 - 191 °C345 - 375 °F
Front Barrel Temperature 179 - 196 °C355 - 385 °F
Nozzle Temperature 185 - 204 °C365 - 400 °F
Mold Temperature 21.1 - 37.8 °C70.0 - 100 °F
Back Pressure 0.345 - 0.689 MPa50.0 - 100 psi
 
Descriptive Properties
Injection RateFast

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
BASF Capron® GR15 15% Glass-Filled Nylon 6 (Dry)
Multibase TPSiV® 3010-50A Thermoplastic Silicone Vulcanizate
ExxonMobil Santoprene® 121-40B260 Thermoplastic Vulcanizate Elastomer
Elastocon TPE Technologies Elastocon® 8088BL Thermoplastic Elastomer
Elastocon TPE Technologies Elastocon® 8068BL Thermoplastic Elastomer

PELASC13 / 81657

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.