MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Evonik Vestodur® X9407 Polymer Modified PBT  (discontinued **)
Categories: Polymer; Thermoplastic; Polyester, TP; Polybutylene Terephthalate (PBT); Polybutylene Terephthalate (PBT), Unreinforced, Molded

Material Notes: Description: VESTODUR X9407 is a special compound polymer modified based on polybutylene terephthalate. The resin is used as an adhesive to bond together VESTAMID(polyamide 12) and VESTODUR (polybutylene terephthalate) in multilayer tubing 1000.1 (MLT 1000.1)developed by Degussa. MLT 1000.1 is a 3-layer-tubing comprising an outermost layer of VESTAMID LX9010, an adhesive layer of VESTODUR X9407, and an innermost layer of VESTODUR X9406. This MLT was developed as fuel line tubing with outstanding resistance against hydrocarbon permeation when alcohol containing fuels are used. VESTODUR X9407 provides excellent bonding between layers consisting of polybutylene terephthalate and polyamide 12 also after contact with fuels at elevated temperatures.

Information provided by degussa.

Evonik Industries is the successor company to Degussa.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.13 g/ccISO 1183
Melt Flow 18.08 g/10 min
@Load 2.16 kg,
Temperature 250 °C
ISO 1133
 50.85 g/10 min
@Load 5.00 kg,
Temperature 250 °C
ISO 1133
 158.2 g/10 min
@Load 10.0 kg,
Temperature 260 °C
ISO 1133
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength, Yield 40.0 MPaISO 527-1/2
Elongation at Break >= 50 %ISO 527-1/2
Elongation at Yield 7.0 %ISO 527-1/2
Tensile Modulus 1.50 GPaISO 527-1/-2
Charpy Impact Unnotched NB
@Temperature -30.0 °C
ISO 179/1eU
 NB
@Temperature 23.0 °C
ISO 179/1eU
Charpy Impact, Notched 1.00 J/cm²
@Temperature -30.0 °C
ISO 179/1eA
 1.20 J/cm²
@Temperature 23.0 °C
ISO 179/1eA
 
Thermal PropertiesOriginal ValueComments
CTE, linear 120 µm/m-°C
@Temperature 23.0 - 80.0 °C
Longitudinal; ISO 11359, DIN 53752
CTE, linear, Transverse to Flow 120 µm/m-°C
@Temperature 23.0 - 80.0 °C
ISO 11359, DIN 53752
Deflection Temperature at 0.46 MPa (66 psi) 130 °CISO 75-1/-2
Deflection Temperature at 1.8 MPa (264 psi) 50.0 °CISO 75-1/-2
Vicat Softening Point 135 °CMethod B, 50 N; ISO 306
 180 °CMethod A, 10 N; ISO 306

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Evonik Vestodur® X9406 Black E70167 Impact Modified PBT
Evonik VESTAMID® MLT 1000.1 Nonconductive multi-layer tubes
Evonik Vestodur® 3000 High Viscosity PBT

PHUMA76 / 47590

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.