MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

(Viewing data as-entered. Click here to return)
Röchling Glastic BMC 1423 GTP Glass-Reinforced Polyester  (discontinued **)
Categories: Polymer; Thermoset; Filled/Reinforced Thermoset; Polyester, TS; Thermoset Polyester Glass Filled BMC

Material Notes: Data provided by Glastic Corporation.

Wear resistant electrical grade.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.846 g/ccASTM D792
Water Absorption 0.184 %ASTM D570
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength, Ultimate 47.0 MPaASTM D638
Tensile Modulus 12.0 GPaASTM D638
Flexural Strength 112 MPaASTM D790
Flexural Modulus 10.0 GPaASTM D790
Compressive Strength 135 MPaASTM D695
Shear Strength 41.0 MPaASTM D732
Izod Impact, Notched 2.10 J/cmASTM D256
 
Electrical PropertiesOriginal ValueComments
Surface Resistance 1.79e+15 ohmInsulation Resistance, Condition A, ASTM D257
Dielectric Constant 4.4
@Frequency 1e+6 Hz
Condition A, ASTM D150
 5.3
@Frequency 60 Hz
Condition A, ASTM D150
Dielectric Strength 17.0 kV/mmShort-Term, ASTM D149
Dissipation Factor 0.015
@Frequency 1e+6 Hz
Condition A, ASTM D150
 0.017
@Frequency 60 Hz
Condition A, ASTM D150; ASTM D150
Arc Resistance 189 secASTM D495
 
Thermal PropertiesOriginal ValueComments
Deflection Temperature at 1.8 MPa (264 psi) >= 260 °CASTM D648
UL RTI, Electrical 130 °CUL 746B
UL RTI, Mechanical with Impact 130 °CUL 746B
Flammability, UL94 V-0

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Röchling Glastic Laminates/Shapes Polyester, Channels and Structural Shapes (GPO3)
Röchling Glastic BMC SLC-2000 Glass-Reinforced Polyester, Compression Molded
Röchling Glastic BMC 1403 GTP Glass-Reinforced Polyester
Röchling Glastic BMC 1401 GTP Glass-Reinforced Polyester

PGLAS4 / 41905

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.