MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Ensinger PEI

Go Yen Chemical Goyenchem-TPI 35 High Effective Phosphoric Acid Flame Retardant
Categories: Other Engineering Material; Additive/Filler for Polymer

Material Notes: Goyenchem-TPI series is an Triaryl phosphate isopropylated flame retardant. With high effective flame retardant ability, it is wildly used in fabric coating, various kinds of resins, PVC, flexible polyurethane and synthetic rubber etc.

Intro: GO YEN CHEMICAL INDUSTRIAL CO., LTD (GYC Group) is the biggest fine chemical manufacture in Asia and has remarkable R&D team. Goyenchem-TPI series is an Triaryl phosphate isopropylated flame retardant. With high effective flame retardant ability, it is wildly used in fabric coating, various kinds of resins, PVC, flexible polyurethane and synthetic rubber etc.

Applications:

  • various thermolplastic and thermolsetting resins
  • variousengineering resins, such asmodified PPO, polycarbonate, polycarbonate blends
  • variousPVCflame retardant application
  • additive for variousoil product
  • various kinds ofresin, such asphenolic resin and cellulosic resin etc.
  • flexible polyurethane
  • synthetic rubber
  • fabric coating
  • various special high valued application

Information provided by Go Yen Chemical

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.183 g/cc0.04274 lb/in³
Viscosity 42 - 50 cP42 - 50 cP
 
Chemical PropertiesMetricEnglishComments
Acid Value <= 0.10<= 0.10mgKOH/g
 
Thermal PropertiesMetricEnglishComments
Flash Point >= 220 °C>= 428 °F
 
Processing PropertiesMetricEnglishComments
Moisture Content <= 0.10 %<= 0.10 %
 
Component Elements PropertiesMetricEnglishComments
Phosphorus, P 8.6 %8.6 %
 
Descriptive Properties
AppearanceAchromatic or light yellow transparent liquid
Color<50APHA

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PGOYEN171 / 266479

Visit Zeus Inc. for PEEK Tubing

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.