MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

Shinkong Synthetic Fibers Shinite® E202G30 PBT, 30% Glass Filled
Categories: Polymer; Thermoplastic; Polyester, TP; Polybutylene Terephthalate (PBT); Polybutylene Terephthalate (PBT), 30% Glass Fiber Filled

Material Notes:

Information from Shinkong Synthetic Fibers Corp.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 1.61 g/cc1.61 g/ccASTM D792
Water Absorption 0.070 %0.070 %ASTM D570
Linear Mold Shrinkage, Flow 0.0020 - 0.0040 cm/cm0.0020 - 0.0040 in/inASTM D955
Linear Mold Shrinkage, Transverse 0.0050 - 0.0090 cm/cm0.0050 - 0.0090 in/inASTM D955
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength 127 MPa18500 psiASTM D638
Elongation at Break 3.0 %3.0 %ASTM D638
Flexural Yield Strength 196 MPa28400 psiASTM D790
Flexural Modulus 9.12 GPa1320 ksiASTM D790
Izod Impact, Notched 0.883 J/cm
@Thickness 3.17 mm,
Temperature 23.0 °C
1.65 ft-lb/in
@Thickness 0.125 in,
Temperature 73.4 °F
ASTM D256
 
Electrical PropertiesMetricEnglishComments
Volume Resistivity 1.00e+16 ohm-cm1.00e+16 ohm-cmASTM D257
Dielectric Constant 4.04.0ASTM D150
Dielectric Strength 33.0 kV/mm838 kV/inASTM D149
 
Thermal PropertiesMetricEnglishComments
Deflection Temperature at 1.8 MPa (264 psi) 210 °C410 °FASTM D648
Flammability, UL94 V-0V-0

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Overview of materials for Polybutylene Terephthalate (PBT), 30% Glass Fiber Filled
Celanese Celanex® 3316 PBT, 30% Glass Reinforced
Avient Edgetek® NT-30GF/000 Nylon 6/6, Glass Filled
Kuraray Genestar™ GN2330 Nylon, 33% Glass Filled
DuPont Mobility and Materials Zytel® 70G30HSL NC010 PA66-GF30

PSHNK008 / 120778

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.