MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Elmet Technologies

Hexcel® TP-2000 Thermoplastic Polyurethane-based MAGRAM Absorber
Categories: Polymer; Thermoplastic; Polyurethane, TP

Material Notes: Description:
  • MAGRAM absorber that utilizes a thermoplastic polyurethane binder to provide a good balance of mechanical, thermal, and electrical properties.
  • This product line is designed for attenuation in the range below 5 GHz.
  • Performance can be tailored to specific applications.
  • Ideally suited as a near-field absorber/suppressor in electronic enclosures.
  • Custom sheet sizes available up to 24” x 48”(60.96 cm x 121.92 cm) ranging in thickness from0.010” to 0.100” (0.254 mm to 2.54 mm)
  • Custom parts can be injection molded in a wide variety of shapes and sizes
  • Halogen free, RoHS and REACH compliant.

Information provided by Hexcel Corporation.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore D 75.075.0ASTM D2240
Tensile Strength 17.2 MPa2500 psiASTM D638
Elongation at Break 28.0 %28.0 %ASTM D638
Tensile Modulus 0.400 GPa58.0 ksiASTM D638
Flexural Modulus 0.820 GPa119 ksiASTM D790
Izod Impact, Notched 0.240 J/cm0.450 ft-lb/inASTM D256
Izod Impact, Unnotched 1.19 J/cm2.23 ft-lb/inASTM D4812
 
Electrical PropertiesMetricEnglishComments
Surface Resistivity per Square >= 2.00e+9 ohm>= 2.00e+9 ohmASTM D257
 
Thermal PropertiesMetricEnglishComments
Thermal Conductivity 1.31 W/m-K9.09 BTU-in/hr-ft²-°FASTM E1530
 
Descriptive Properties
ColorBlack

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PHEXCB9585 / 322739

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.