MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Metalmen Sales

(Viewing data as-entered. Click here to return)
Nitronic 40 Stainless Steel Plate
Categories: Metal; Ferrous Metal; Stainless Steel

Material Notes: Electroslag remelted; as-rolled

Vendors: Visit metalmen for your metals needs. Products include special chemistry, tight tolerances, custom tempers, odd dimensions/forms, and small quantities. Phone 1-800-767-9494.

Click here to view all available suppliers for this material.

Please click here if you are a supplier and would like information on how to add your listing to this material.

 
Mechanical PropertiesOriginal ValueComments
Tensile Strength 1010 MPa
@Temperature 23.0 °C
 1170 MPa
@Temperature -73.3 °C
 1830 MPa
@Temperature -196 °C
Tensile Strength, Yield 840 MPa
@Temperature 23.0 °C
 945 MPa
@Temperature -73.3 °C
 1540 MPa
@Temperature -196 °C
Elongation at Break 31 %
@Temperature -196 °C
 35 %
@Temperature 23.0 °C
 36 %
@Temperature -73.3 °C
Reduction of Area 64 %
@Temperature -196 °C
 71 %
@Temperature -73.3 °C
 72 %
@Temperature 23.0 °C

References for this datasheet.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
MetalTek Nitronic® 40 Austenitic Stainless Steel
HP Alloys Nitronic® 60 Austenitic Stainless, Annealed
MetalTek Nitronic® 60 Cast UNS J92972 Austenitic Stainless Steel
AISI 4140 Steel, normalized at 870°C (1600°F), air cooled, 13 mm (0.5 in.) round
Mi-Tech Metals HD17 Tungsten-Based Metal

MQZ9935 / 172185

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.