MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Elmet Technologies

(Viewing data as-entered. Click here to return)
Polygon Composites Polygon Tube® Double Insulation Tubing
Categories: Other Engineering Material

Material Notes: The Polygon Tube® is the insulation sleeve that provides armatures of electric motors a secondary layer of insulation. This secondary insulation is needed to provide increased protection for operators of electrical appliances from shock. The use of the additional layer of insulation allows the appliance to be rated “Double Insulated” and the need for grounding of the appliance is eliminated. Even though an appliance is grounded by means of a three-wire power cord, it is still a good practice to provide a secondary layer of insulation. The information provided is to assist in the design and assembly of the Polygon Tube into armatures of electric motors.

Information provided by Polygon

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 1.80 g/cc
Water Absorption 0.12 %
@Time 7200 sec
 0.16 %
@Time 86400 sec
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength 20.0 ksiGeneral
Compressive Strength 20000 psi
Shear Strength 6500 psi
 
Electrical PropertiesOriginal ValueComments
Volume Resistivity 2.41e+18 ohm-cm
Surface Resistance 3.93e+15 ohm
Insulation Resistance 2.38e+12 ohm
@Thickness 203 mm
Dielectric Constant 4.15
@Frequency 60 Hz
Dielectric Strength 400 V/mil
Dissipation Factor 0.0094
@Frequency 60 Hz

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Morgan Advanced Ceramics TR® 2000SL Thermal Ceramic

PPOLYG10 / 184509

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.