MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Zoltek™ OX FT1700-110 Oxidized PAN Fiber Felt
Categories: Carbon; Carbon Fiber/Carbon Fibre; Other Engineering Material; Composite Fibers

Material Notes: Produced from 100% ZOLTEK OX oxidized PAN fibers, needlepunched felts are for use as thermal/acoustical insulation in aerospace, automotive or general industrial high temperature applications. Valuable as a low cost - high performance fire or spark barrier.

Information provided by Zoltek Corporation.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.36 g/cc
Thickness 12700 micronsCured
 
Electrical PropertiesOriginal ValueComments
Electrical Resistivity 8.00e+8 ohm-cm
 
Thermal PropertiesOriginal ValueComments
Oxygen Index >= 40 %
 
Component Elements PropertiesOriginal ValueComments
Carbon, C 62 %
Hydrogen, H 4.5 %
Nitrogen, N 21.5 %
O2 12 %
Sodium, Na <= 0.10 %
Trace Metals <= 0.010 %
 
Descriptive Properties
Areal Weight1700 g/m2. ( custom weights available)
ColorBlack
Fiber Diameter (µm)12.5
Fiber Input1.7 or 2.2 dTex.
Organic SolventsExcellent resistance
Roll Length60m.
Roll Width117cm.
Strong AcidsGood resistance
Strong BasesPoor resistance
Weak AcidsExcellent resistance
Weak BasesGood resistance

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
DowAksa AKSACA™ A-38 3K Continuous Carbon Fiber
Graphite, Carbon, C
Hexcel® HexTow® AS4C 3K Standard Modulus Carbon Fiber (3000 Filaments)
Aremco Graphi-Bond™ 551-R
Aremco Graphi-Bond™ 551-RN High Temperature Ceramic Adhesive/Paste, Graphite Filled

ECZO832i / 232307

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.