HG3457 is produced by gas phase polymerization. This nominal 18 melt flow index product is specifically designed for fiber applications requiring good melt, UV and thermal stability in the finished product. Specific applications include carpet face yarn, industrial fabrics and geotextiles. This material meets Food and Drug Administration requirements of 21CFTR 177.1520. |