MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
3M Scotch-Weld™ 1099-L Nitrile High Performance Plastic Adhesives
Categories: Polymer; Adhesive

Material Notes:

Features:

  • It is a low viscosity grade for spray application.
  • Fast drying
  • Provides strong, flexible bonds.
  • Resists weathering, water, fuels, oil and plasticizers.
  • Bonds vinyl extrusions and sheeting. (May stain light colored vinyls.)
  • Also bonds fabrics, foams and many plastics. (Not recommended for polyolefin plastic bonding)
  • May be heat cured to obtain superior physical properties

Information provided by 3M

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Solids Content 22 - 26 %
Brookfield Viscosity 200 - 325 cPRVF #2 sp @ 20 rpm
 
Mechanical PropertiesOriginal ValueComments
Shear Strength 467 psi
@Temperature 121 °C
Overlap, 1/8" Alum/Alum
 607 psi
@Temperature 93.0 °C
Overlap, 1/8" Alum/Alum
 643 psi
@Temperature 82.0 °C
Overlap, 1/8" Alum/Alum
 897 psi
@Temperature 65.0 °C
Overlap, 1/8" Alum/Alum
 1306 psi
@Temperature 24.0 °C
Overlap, 1/8" Alum/Alum
 2989 psi
@Temperature -55.0 °C
Overlap, 1/8" Alum/Alum
 3409 psi
@Temperature -34.0 °C
Overlap, 1/8" Alum/Alum
Peel Strength 3.50 pli
@Temperature 82.0 °C,
Time 1.81e+6 sec
180°, Canvas/Steel
 7.00 pli
@Temperature 66.0 °C,
Time 1.81e+6 sec
180°, Canvas/Steel
 16.5 pli
@Temperature 24.0 °C,
Time 86400 sec
180°, Canvas/Steel
 17.5 pli
@Temperature -34.0 °C,
Time 1.81e+6 sec
180°, Canvas/Steel
 23.5 pli
@Temperature 24.0 °C,
Time 432000 sec
180°, Canvas/Steel
 26.0 pli
@Temperature 24.0 °C,
Time 259000 sec
180°, Canvas/Steel
 27.5 pli
@Temperature 24.0 °C,
Time 605000 sec
180°, Canvas/Steel
 30.0 pli
@Temperature 24.0 °C,
Time 1.81e+6 sec
180°, Canvas/Steel
 31.0 pli
@Temperature 24.0 °C,
Time 1.21e+6 sec
180°, Canvas/Steel
 
Thermal PropertiesOriginal ValueComments
Flash Point -18.0 °CTCC
 
Descriptive Properties
AppearanceLight tan
BaseNitrile Rubber

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Lord Adhesives HPC-5B Hydrogenated Nitrile Butadiene Rubber Coating
3M Scotch-Weld™ 4491 Nitrile Industrial Adhesive
3M Scotch-Weld™ 1099 Nitrile High Performance Plastic Adhesives
3M Scotch-Weld™ 826 Nitrile Rubber & Plastic Adhesive
Lord Adhesives HPC-5C Hydrogenated Nitrile Butadiene Rubber Coating

PMM34118 / 168865

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.