MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Sumitomo Bakelite Durez® P23056NF Phenolic Resin
Categories: Polymer; Thermoset; Phenolic

Material Notes: Plyophen® 23056 NF is a phenolic resole type of resin diluted in ethanol. This resin is designed for impregnation of fabrics, such as paper, glass fibers and Nomex. The resin provides exceptional mechanical and chemical resistance properties to the finished laminates.

Information provided by Sumitomo Bakelite High Performance Plastics (sbhpp)

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Solids Content 63 %
@Load 0.00100 kg,
Temperature 135 °C
63 %
@Load 0.00221 lb,
Temperature 275 °F
3h; DCT 156
Viscosity 850 cP
@Temperature 25.0 °C
850 cP
@Temperature 77.0 °F
DCT 61
 
Processing PropertiesMetricEnglishComments
Cure Time 1.17 min
@Temperature 152 °C
0.0194 hour
@Temperature 306 °F
DCT 162.152

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Sumitomo Bakelite Durez® 10694 Phenolic Resin
Sumitomo Bakelite Plyophen 23900 Phenolic Resin
Sumitomo Bakelite Plyophen 23057 Phenolic Resin

PSUMIT180 / 193985

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.