MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

(Viewing data as-entered. Click here to return)
Celanese Zytel® LC6200 BK385 PA612-HI
Categories: Polymer; Thermoplastic; Nylon (Polyamide PA); Nylon 612 (PA612); Nylon 612, Impact Modified

Material Notes: Toughened Polyamide 612 Developed for Extrusion

Former DuPont product acquired by Celanese in 2022.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.00 g/ccDAM; ISO 1183
Melt Density 0.820 g/cc
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength, Yield 29.2 MPa50% RH; ISO 527-1/-2
 32.2 MPaDAM; ISO 527-1/-2
Elongation at Yield 13 %DAM; ISO 527-1/-2
 22 %50% RH; ISO 527-1/-2
Tensile Modulus 720 MPa50% RH; ISO 527-1/-2
 1080 MPaDAM; ISO 527-1/-2
Poissons Ratio 0.45DAM
 0.4650% RH
Izod Impact, Notched (ISO) 13.0 kJ/m²
@Temperature -30.0 °C
50% RH; ISO 180/1A
 13.0 kJ/m²
@Temperature -30.0 °C
DAM; ISO 180/1A
 27.0 kJ/m²
@Temperature 23.0 °C
DAM; ISO 180/1A
 66.0 kJ/m²
@Temperature 23.0 °C
50% RH; ISO 180/1A
Charpy Impact, Notched 15.0 kJ/m²
@Temperature -30.0 °C
50% RH; ISO 179/1eA
 15.0 kJ/m²
@Temperature -30.0 °C
DAM; ISO 179/1eA
 40.0 kJ/m²
@Temperature 23.0 °C
DAM; ISO 179/1eA
 80.0 kJ/m²
@Temperature 23.0 °C
50% RH; ISO 179/1eA
Abrasion 12mm3; DAM; ISO 4649
 
Thermal PropertiesOriginal ValueComments
Specific Heat Capacity 2.70 J/g-°CMelt
Thermal Conductivity 0.170 W/m-KMelt
Melting Point 218 °C10°C/min; DAM; ISO 11357-1/-3
Deflection Temperature at 0.46 MPa (66 psi) 85.0 °CDAM; ISO 75-1/-2
Deflection Temperature at 1.8 MPa (264 psi) 46.0 °CDAM; ISO 75-1/-2
Flame Spread <= 80.0 mm/min
@Thickness 1.00 mm
ISO 3795 (FMVSS 302)
 
Processing PropertiesOriginal ValueComments
Melt Temperature 240 °COptimum, Extrusion
 235 - 250 °CRange, Extrusion
Drying Temperature 75.0 - 80.0 °CExtrusion
Dry Time 3.00 - 4.00 hourExtrusion, Dehumidified Dryer
Moisture Content <= 0.060 %Extrusion
 
Descriptive Properties
FMVSS ClassBISO 3795 (FMVSS 302)
ISO designationISO 16396-PA612-I,,M1CG1H,S18-010
Part Marking Code>PA612-HI<ISO 11469
PolymerPA612
Resin IdentificationPA612-HIISO 1043

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Celanese Zytel® 151L NC010 PA612
Evonik Vestamid® D16 Nylon 612 (Dry as Molded)
Celanese Zytel® LC6210 BK010 PA612-HI
Celanese Zytel® 77G33L BK031 PA612-GF33
Celanese Zytel® 153HSL NC010 PA612

PDSX5474 / 198114

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.