MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

Westlake EB169 Low Density Polyethylene  (discontinued **)
Categories: Polymer; Thermoplastic; Polyethylene (PE); Low Density (LDPE)

Material Notes: Westlake EB169 is a low-density polyethylene with high stiffness designed for beverage shrink overwrap and towel/tissue packaging. It has good toughness and blends well with LLDPE resins.

    Application/Uses
  • Beverage overwrap shrink film
  • Light and medium duty produce bags
  • Clarity packaging

FDA: This material complies with FDA regulations in 21 CFR, section 177.1520. Kosher Compliant.

All information provided by Westlake Chemical

Key Words: Good toughness and blends well with LLDPE resins
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 0.927 g/cc0.0335 lb/in³ASTM D1505
Thickness 31.8 microns1.25 mil
Melt Flow 1.6 g/10 min1.6 g/10 minASTM D1238
 
Mechanical PropertiesMetricEnglishComments
Film Elongation at Break, MD 300 %300 %ASTM D882
Film Elongation at Break, TD 800 %800 %ASTM D882
Dart Drop 3.35 g/micron85.0 g/milASTM D1709
Film Tensile Strength at Break, MD 19.3 MPa2800 psiASTM D882
Film Tensile Strength at Break, TD 17.9 MPa2600 psiASTM D882
1% Secant Modulus, MD 234 MPa34000 psiASTM D882
1% Secant Modulus, TD 276 MPa40000 psiASTM D882
 
Optical PropertiesMetricEnglishComments
Haze 6.5 %6.5 %ASTM D1003
Gloss 65 %65 %at 45º; ASTM D2457
 
Processing PropertiesMetricEnglishComments
Melt Temperature 182 - 199 °C360 - 390 °Fwith BUR of 1.5:1 or higher
Blow-up Ratio (BUR) 2.52.5
 
Descriptive Properties
ProcessFilm

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Westlake Hifor Xtreme SC74838 Linear Low Density Polyethylene
Westlake Hifor SC74561-F Clear (Voridian) Polyethylene Film, Using Energx Technology Services
Westlake Hifor LT74107-F Polyethylene Film, Using Energx Technology Services
Westlake EC477AA Low Density Polyethylene
Westlake EC476AA Low Density Polyethylene

PWESF030 / 84467

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.