MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Ensinger PEI

NOVA Chemicals EPS M77BG Expanded Polystyrene
Categories: Polymer; Thermoplastic; Polystyrene (PS); Expanded Polystyrene (EPS)

Material Notes: EPS has excellent physical properties, low energy consumption and has FDA compliant offerings. Its lightweight and proven performance makes it suitable for a wide variety of markets and applications including building & construction, geofoam, packaging, and cup & container. EPS enable customers to produce high-quality products that are sturdy, safe and durable. Features/Attributes: Low Density Potential, Controlled/Uniform, Expansion. Applications: Insulation, SIP's, Fabricated Packaging.

Information provided by NOVA Chemicals.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Bulk Density 0.609 - 0.641 g/cc0.0220 - 0.0231 lb/in³
Volatiles 6.5 %6.5 %Pentane, by weight
Bead Size 0.850 mm0.0335 inaverage size
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength 0.414 MPa60.0 psi@ 2 pcf; MIL-P-19644
 0.758 MPa110 psi@ 3.5 pcf; MIL-P-19644
 1.10 MPa160 psi@ 5 pcf; MIL-P-19644
Flexural Strength 0.138 MPa20.0 psi@ 1 pcf; ASTM C203
 0.758 MPa110 psi@ 3.5 pcf; ASTM C203
 1.14 MPa165 psi@ 5 pcf; ASTM C203
Compressive Strength  0.0621 MPa
@Strain 10 %
9.00 psi
@Strain 10 %
@ 1 pcf; ASTM D-1621
 0.207 MPa
@Strain 10 %
30.0 psi
@Strain 10 %
@ 2 pcf; ASTM D-1621
 0.276 MPa
@Strain 10 %
40.0 psi
@Strain 10 %
@ 2.5 pcf; ASTM D-1621
 
Thermal PropertiesMetricEnglishComments
CTE, linear 63.0 µm/m-°C35.0 µin/in-°F
Thermal Conductivity 0.0303 - 0.0346 W/m-K0.210 - 0.240 BTU-in/hr-ft²-°FK-factor, Lambda
 0.0339 W/m-K0.235 BTU-in/hr-ft²-°F@ 2.5 pcf; ASTM C-518
 0.0344 W/m-K0.239 BTU-in/hr-ft²-°F@ 2.0 pcf; ASTM C-518
 0.0349 W/m-K0.242 BTU-in/hr-ft²-°F@ 1.5 pcf; ASTM C-518
 0.0352 W/m-K0.244 BTU-in/hr-ft²-°F@ 1.25 pcf; ASTM C-518
 0.0360 W/m-K0.250 BTU-in/hr-ft²-°F@ 1.0 pcf; ASTM C-518
Insulation R Value 3.9 - 4.23.9 - 4.2per inch
Maximum Service Temperature, Air 79.4 °C175 °F
 
Descriptive Properties
Water Absorbed0.03 lb/ft²@ 5 pcf MIL P 19644
 0.04 lb/ft²@ 1.5 pcf MIL P 19644
 0.04 lb/ft²@ 2.0 pcf MIL P 19644
 0.04 lb/ft²@ 2.5 pcf MIL P 19644
 0.04 lb/ft²@ 3.0 pcf MIL P 19644
 0.05 lb/ft²@ 1 pcf. MIL P 19644
Water Vapor Permeability (in)0.5 - 1.5ASTM C355. Plaques. Optimum fusion. 2.2 pcf
 0.5 - 1.5ASTM C355. Plaques. Optimum fusion. 2.5 pcf
 0.5 - 2.0ASTM C355. Plaques. Optimum fusion. 1.4 pcf
 1.0-2.0ASTM C355. Plaques. Optimum fusion. 1.0 pcf
 1.0-2.0ASTM C355. Plaques. Optimum fusion. 2.3 pcf
 1.5-3.0ASTM C355. Plaques. Optimum fusion. 1.0 pcf

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PNOV623 / 249078

Visit Zeus Inc. for PEEK Tubing

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.