MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

NOVA Chemicals SURPASS® FPs016-A LLDPE
Categories: Polymer; Thermoplastic; Polyethylene (PE); Linear Low Density (LLDPE); Linear Low Density Polyethylene (LLDPE), Extrusion Grade

Material Notes: Availability: North America

Additive: Processing Stabilizer

Features: Copolymer; Food Contact Acceptable; Good Melt Strength; Good Tear Strength; Good Toughness; Low Density; Low Gel; Octene Comonomer

Uses: Film; Laminates

Agency Ratings: FDA 21 CFR 177.1520©3.2a

Form: Pellets

Processing Method: Coextrusion; Film Extrusion

Information provided by NOVA Chemicals

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 0.918 g/cc0.0332 lb/in³ASTM D792
Melt Flow 0.65 g/10 min
@Load 2.16 kg,
Temperature 190 °C
0.65 g/10 min
@Load 4.76 lb,
Temperature 374 °F
ASTM D1238
 
Mechanical PropertiesMetricEnglishComments
Film Tensile Strength at Yield, MD 8.48 MPa
@Thickness 0.0249 mm
1230 psi
@Thickness 0.000980 in
Blown Film; ASTM D882
Film Tensile Strength at Yield, TD 8.48 MPa
@Thickness 0.0249 mm
1230 psi
@Thickness 0.000980 in
Blown Film; ASTM D882
Film Elongation at Break, MD 470 %
@Thickness 0.0249 mm
470 %
@Thickness 0.000980 in
Blown Film; ASTM D882
Film Elongation at Break, TD 780 %
@Thickness 0.0249 mm
780 %
@Thickness 0.000980 in
Blown Film; ASTM D882
Elmendorf Tear Strength MD 350 g
@Thickness 0.0249 mm
350 g
@Thickness 0.000980 in
Blown Film; ASTM D1922
Elmendorf Tear Strength TD 430 g
@Thickness 0.0249 mm
430 g
@Thickness 0.000980 in
Blown Film; ASTM D1922
Dart Drop Test 700 g
@Thickness 0.0249 mm
1.54 lb
@Thickness 0.000980 in
Blown Film, F50; ASTM D1709A
Film Tensile Strength at Break, MD 47.0 MPa
@Thickness 0.0249 mm
6820 psi
@Thickness 0.000980 in
Blown Film; ASTM D882
Film Tensile Strength at Break, TD 44.0 MPa
@Thickness 0.0249 mm
6380 psi
@Thickness 0.000980 in
Blown Film; ASTM D882
Heat Seal Strength Initiation Temperature 100 °C212 °F0.98 mil, Blown Film
 
Optical PropertiesMetricEnglishComments
Haze  7.0 %
@Thickness 0.0249 mm
7.0 %
@Thickness 0.000980 in
Blown Film, LLDPE Blended; ASTM D1003
 15 %
@Thickness 0.0249 mm
15 %
@Thickness 0.000980 in
Blown Film, 100% LLDPE; ASTM D1003
Gloss  38 %
@Thickness 0.0249 mm
38 %
@Thickness 0.000980 in
45°, Blown Film, 100% LLDPE; ASTM D2457
 72 %
@Thickness 0.0249 mm
72 %
@Thickness 0.000980 in
45°, Blown Film, LLDPE Blended; ASTM D2457
 
Processing PropertiesMetricEnglishComments
Melt Temperature 185 - 220 °C365 - 428 °FExtrusion
Blow-up Ratio (BUR) 2.0 - 3.52.0 - 3.5
 
Descriptive Properties
Low Friction Puncture22.0 in-lb/milBlown Film (1.0 mil)

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PNOVC802 / 311495

Master Bond adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.