MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

Taiwan PU TXS450612-7 PU Disc
Categories: Polymer; Thermoplastic; Polyurethane, TP

Material Notes: Key features:
  • Very high wear resistance under high speed rotation
  • High abrasion resistance
  • Various in hardness for different yarn qualities and deniers
  • Long life cycle
Application: PU Disc can use for transmission of textile machinery, whole plant equipment, shoe machinery, watch making machinery and so on.

Information provided by Taiwan PU Corporation

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 1.06 g/cc1.06 g/cc
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore A 9090
Tensile Strength 43.5 MPa6310 psi
Elongation at Break 480 %480 %
100% Modulus 8.35 MPa1210 psi
300% Modulus 14.4 MPa2090 psi
Rebound 46 %46 %Bashore
Tear Strength 17.5 kN/m100 pliDie C; ASTM D1938
 43.8 kN/m250 pliDie C; ASTM D624
Compression Set 34 %
@Temperature 21.1 °C,
Time 79200 sec
34 %
@Temperature 70.0 °F,
Time 22.0 hour
 
Thermal PropertiesMetricEnglishComments
Brittleness Temperature >= 62.0 °C>= 144 °FBell

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PTAIWPU493 / 306223

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.