MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Specialty Compounds RTP Company

Lotte Advanced Materials TITANEX HM4560UA HDPE, Blow Molding
Categories: Polymer; Thermoplastic; Polyethylene (PE); High Density (HDPE); High Density Polyethylene (HDPE), Extruded

Material Notes: HM4560UA is an UV light stabilized, pelleted high molecular weight, high density polyethylene Hexene-1 resin for medium-large blow molding.

Applications: Intermediate bulk containers, agricultural containers, industrial chemical containers and pallets.

Advantages: Excellent stress crack resistance, excellent resistance to most chemicals and outstanding rigidity with high impact strength and high melt strength.

Information provided by Lotte Advanced Materials.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 0.945 g/cc0.0341 lb/in³ASTM D1505
ESCR 10% Igepal® >= 1000 hour>= 1000 hourF50; ASTM D1693
Melt Flow 6.00 g/10 min6.00 g/10 minI21; ASTM D1238
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength at Break 350 MPa50800 psiASTM D638
Tensile Strength, Yield 23.5 MPa3410 psiASTM D638
Elongation, Ultimate >= 600 %>= 600 %ASTM D638
Flexural Modulus 1.08 GPa156 ksiASTM D790
Izod Impact, Notched 6.37 J/cm11.9 ft-lb/inASTM D256
 
Thermal PropertiesMetricEnglishComments
Deflection Temperature at 0.46 MPa (66 psi) 75.0 °C167 °FASTM D648
Vicat Softening Point 125 °C257 °FASTM D1525
 
Processing PropertiesMetricEnglishComments
Processing Temperature 180 - 220 °C356 - 428 °FRear zone temperature setting
 190 - 230 °C374 - 446 °FFront zone temperature setting
Die Temperature 190 - 230 °C374 - 446 °F
Head Temperature 190 - 230 °C374 - 446 °F

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PLOTT9600 / 326082

Visit Zeus Inc. for PEEK Tubing

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.