MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
NovaCentrix Metalon® JS-B25HV Nanosilver Ink – Aqueous dispersion for Dimatix Printheads
Categories: Fluid; Other Engineering Material

Material Notes: JS-B25HV is an electrically conductive ink designed to produce circuits on porous and non-porous substrates including inkjet papers, PET, polyimide, and glass. JS-B25HV ink is specially formulated for compatibility and stability with Dimatix printheads. A printing waveform for Dimatix DMP heads is available.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 1.30 g/cc
Particle Size 60 µmz-avg by DLS
Viscosity 8.0 cP
Surface Tension 30 - 32 dynes/cm
 
Electrical PropertiesOriginal ValueComments
Volume Resistivity 0.0000028 ohm-cmExample; on coated PET substrate
Surface Resistivity per Square 0.050 ohmExample; on coated PET substrate
 
Component Elements PropertiesOriginal ValueComments
Silver, Ag 25 %

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
SunChemical Gwent C2020624D2 Silver Carbon Ink
SunChemical Gwent C2020522D1 Silver Ink
NovaCentrix PSI-219® Conductive Screen Ink
NovaCentrix PSI-211® Conductive Screen Ink
NovaCentrix Metalon® JS-B40G Nanosilver Ink – Aqueous dispersion for Dimatix Printheads

ENOVA907 / 191517

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.