MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

Eastman Therminol 55 Heat Transfer Fluid
Categories: Fluid

Material Notes: Therminol 55 is a synthetic heat transfer fluid used in moderate temperature applications. Therminol 55 fluid is designed for use in non-pressurized /low-pressure, indirect heating systems. It delivers efficient, dependable, uniform process heat with no need for high pressures.

Information provided by Eastman

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 0.883 g/cc0.0319 lb/in³Liquid; ASTM D4052
Kinematic Viscosity at 40°C (104°F) 19 cSt19 cStASTM D445
Kinematic Viscosity at 100°C (212°F) 3.52 cSt3.52 cStASTM D445
Molecular Weight 320 g/mol320 g/mol
 
Electrical PropertiesMetricEnglishComments
Dielectric Constant 2.232.23ASTM D924
 
Thermal PropertiesMetricEnglishComments
Heat of Vaporization 228 J/g98.1 BTU/lbat max. use temperature
Boiling Point 351 °C664 °F
Pour Point -54.0 °C-65.2 °FISO 3016
Flash Point 177 °C351 °FCOC; ASTM D92
 
Descriptive Properties
AppearanceClear yellow liquid

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PEATM5610 / 222804

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.