MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Metal adhesives

Parker Chomerics CHO-SHIELD® 4998 Conductive Flexible Coating
Categories: Polymer; Adhesive

Material Notes: Description: CHO-SHIELD® 4998 is a smooth, highly conductive flexible silver-filled polyurethane coating designed for military/aerospace airframe applications. Both coatings provide superior adhesion, excellent solvent rub and wear resistance, and are resistant against numerous operational and environmental fluids. CHO-SHIELD® 4498 can be applied to aluminum as well as non-conductive substrates and are designed to be used with primers and with external topcoat systems. CHO-SHIELD® 1091 can be used as a primer for ensuring improved performance on aluminum substrates.

Information provided by Chomerics

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 2.10 g/cc2.10 g/ccWet; ASTM D1475
Volatile Organic Compounds (VOC) Content 596 g/l596 g/lUSEPA Method 24
Thickness 0.0760 - 0.102 microns0.00299 - 0.00402 milRecommended Dry Film
 
Mechanical PropertiesMetricEnglishComments
Impact Test >= 102 J>= 75.0 ft-lbExtrusion; ASTM D2794
 >= 102 J>= 75.0 ft-lbIntrusion; ASTM D2794
Taber Abrasion, mg/1000 Cycles 160160ASTM D4060
 
Electrical PropertiesMetricEnglishComments
Surface Resistivity per Square <= 0.075 ohm<= 0.075 ohmCEPS-0002
 <= 0.075 ohm
@Temperature 22.2 °C,
Time 1.21e+6 sec
<= 0.075 ohm
@Temperature 72.0 °F,
Time 336 hour
MIL-T-5624 JP-8; CEPS-0002
 <= 0.075 ohm
@Temperature 71.1 °C,
Time 605000 sec
<= 0.075 ohm
@Temperature 160 °F,
Time 168 hour
MIL-H-5606 Hydraulic Fluid; CEPS-0002
 <= 0.075 ohm
@Temperature 71.1 °C,
Time 605000 sec
<= 0.075 ohm
@Temperature 160 °F,
Time 168 hour
MIL-L-7808 Lubrication Oil; CEPS-0002
 <= 0.075 ohm
@Temperature 85.0 °C,
Time 1.21e+6 sec
<= 0.075 ohm
@Temperature 185 °F,
Time 336 hour
CEPS-0002
 <= 0.075 ohm
@Temperature -40.0 °C,
Time 1.21e+6 sec
<= 0.075 ohm
@Temperature -40.0 °F,
Time 336 hour
CEPS-0002
 <= 0.075 ohm
@Temperature 85.0 °C,
Time 2.59e+6 sec
<= 0.075 ohm
@Temperature 185 °F,
Time 720 hour
CEPS-0002
Shielding Effectiveness 85 dB
@Frequency 2.00e+8 - 1.00e+10 Hz
85 dB
@Frequency 2.00e+8 - 1.00e+10 Hz
Modified Chomerics TP-08
 
Thermal PropertiesMetricEnglishComments
Maximum Service Temperature, Air 85.0 °C185 °F
Minimum Service Temperature, Air -40.0 °C-40.0 °F
 
Processing PropertiesMetricEnglishComments
Cure Time  120 min
@Temperature 54.0 °C
2.00 hour
@Temperature 129 °F
at Standard Conditions + 2 hrs
 1440 min
@Temperature 15.5 - 21.0 °C
24.0 hour
@Temperature 59.9 - 69.8 °F
40-60% RH
Pot Life 60 min60 minASTM D4212
Shelf Life 6.00 Month6.00 MonthFrom date of Manufacture
 
Descriptive Properties
Adhesion5BASTM D3359
ColorMetallic Light Brown
Conical Bend=>32.0%Cracking: No Evidence; ASTM D522 - Test Method A
Coverage250 sq ft/galat 3.0 mil Dry Film Thickness; Typical; ASTM D2697
Cross Hatch Adhesion5B85°C for 14 days; ASTM D3359
 5B-40°C for 14 days; ASTM D3359
 5B85°C, 85% RH for 30 days; ASTM D3359
FillerSilver
Mandrel Bend>500%ASTM D522 -Test Method B
Mix Ratio100:18.30:1.39:20.57A:B:C:D
ResinPolyurethane
Solvent Rub ResistancePassCHO-TM 95-40-6013
 Pass22.2°C for 14 days; MIL-T-JP-8; CHO-TM 95-40-6013
 Pass71.1°C for 14 days; MIL-H-5606 Hydraulic Fluid; CHO-TM 95-40-6013
 Pass71.1°C for 14 days; MIL-L-7808 Lubrication Oil; CHO-TM 95-40-6013
Visual InspectionPass85°C for 14 days; CHO-TM 95-40-6013
 Pass-40°C for 14 days; CHO-TM 95-40-6013
 Pass85°C, 85% RH for 30 days; CHO-TM 95-40-6013
 Pass22.2°C for 14 days; MIL-T-JP-8; CHO-TM 95-40-6013
 Pass71.1°C for 14 days; MIL-H-5606 Hydraulic Fluid; CHO-TM 95-40-6013
 Pass71.1°C for 14 days; MIL-L-7808 Lubrication Oil; CHO-TM 95-40-6013

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PCHOME233 / 130943

Metal adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.