Low hardness (Duro A 40 >). Natural color cylindrical pellet. Color and hardness are adjustable by compounding with color master batch and PP. Preferable for injection molding. Possible for extrusion molding. Application: Electric tracking prevention seal, Color seal, Orefinic resin modifier, etc. ENEOS has acquired the elastomer product lines from JSR Corporation. |