MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Dowhon DHF-7332F FFKM, Copolymer, Crankshaft oil seal
Categories: Polymer; Thermoset; Fluoropolymer, TS; Thermoset Fluoroelastomer

Material Notes: Property: Good hot tear resistance, good mold release, metal bonding

Information provided by SICHUAN DOWHON NEW MATERIALS CO., LTD.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 1.97 g/cc
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore A 73
 70
@Temperature 150 °C,
Time 252000 sec
OIL 903
 70
@Temperature 23.0 °C,
Time 252000 sec
FUEL C
 74
@Temperature 150 °C,
Time 252000 sec
Engine Oil5W-30
 74
@Temperature 230 °C,
Time 252000 sec
Aging
Tensile Strength 14.82 MPa
 11.767 MPa
@Temperature 150 °C,
Time 252000 sec
Engine Oil5W-30
 12.093 MPa
@Temperature 23.0 °C,
Time 252000 sec
FUEL C
 14.0345 MPa
@Temperature 150 °C,
Time 252000 sec
OIL 903
 15.6203 MPa
@Temperature 230 °C,
Time 252000 sec
Aging
Elongation at Break 210 %
 150.36 %
@Temperature 150 °C,
Time 252000 sec
Engine Oil5W-30
 195.51 %
@Temperature 230 °C,
Time 252000 sec
Aging
 219.66 %
@Temperature 150 °C,
Time 252000 sec
OIL 903
 229.32 %
@Temperature 23.0 °C,
Time 252000 sec
FUEL C
Compression Set 21 %
@Temperature 200 °C,
Time 252000 sec
ASTM D395 Method B
 
Thermal PropertiesOriginal ValueComments
Minimum Service Temperature, Air -17.0 °CTR10
Brittleness Temperature -24.0 °C
 
Descriptive Properties
Colorgreen

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PDOWHON049 / 315961

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.