This gas phase, high molecular weight, homopolymer is tailored for lightweight blow molded applications that:- Require excellent stiffness to ESCR ratio
- Require good melt strength
- Are durable and recyclable for sustainability
Typical blow molded applications for 9518H include: - Household and industrial chemical containers
- Industrial containers / Large parts
This resin meets these specifications: - ASTM D4976 - PE 245
- FDA 21 CFR 177.1520(c) 3.2a, use conditions B through H per 21 CFR 176.170(c)
Information provided by Chevron Phillips Chemical Company LP. |