MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

(Viewing data as-entered. Click here to return)
Chevron Phillips EB6750 Rubber Modified Polystyrene  (discontinued **)
Categories: Polymer; Thermoplastic; Polystyrene (PS); Polystyrene, Impact Modified

Material Notes: Description

Chevron EB6750 is a general purpose, high impact polystyrene material developed for packaging applications. Its processing characteristics make EB6750 suitable for extrusion and deep-draw thermoforming. This material provides good surface smoothness, moderately high heat distortion and excellent practical toughness. Chevron EB6750 natural complies with Food Additive Regulation 21CFR177.1640 for polystyrene and rubber modified polystyrene, which states that such materials may be safely used in contact with foods.

Applications

Chevron EB6750 is recommended for such applications as custom sheet extrusion, cups for hot and cold drinks, conical cup liners, individual portion containers, dairy containers, box liners and medical trays.Information provided by Chevron Phillips Chemical Company.

The Chevron Phillips polystyrene product line was transferred to Americas Styrenics in 2008.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.03 g/ccASTM D792
Melt Flow 3.2 g/10 minCondition G; ASTM D1238
 
Mechanical PropertiesOriginal ValueComments
Hardness, Rockwell R 86ASTM D785
Tensile Strength at Break 2500 psiat 2.0 in/min, Tested using a 50 mil. Sheet; ASTM D638
Tensile Strength, Yield 2300 psiat 2.0 in/min, Tested using a 50 mil. sheet; ASTM D638
Elongation at Break 75 %Tested using a 50 mil. Sheet; ASTM D638
Tensile Modulus 230000 psiTested using a 50 mil. Sheet; ASTM D638
Izod Impact, Notched 1.80 ft-lb/in1/4 in. at 73°F; ASTM D256
 2.10 ft-lb/in1/8 in.; ASTM D256
 1.30 ft-lb/in
@Temperature -17.8 °C
0.125 in (3.2 mm) sample; ASTM D256
 
Thermal PropertiesOriginal ValueComments
Deflection Temperature at 1.8 MPa (264 psi) 185 °FUnannealed specimen; ASTM D648
Vicat Softening Point 212 °FASTM D1525
 
Compliance PropertiesOriginal ValueComments
FDA Yes

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PPSRA15 / 58245

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.