MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Shakespeare Sanstat® CN125 .89mm Nylon 66 Monofilament
Categories: Polymer; Thermoplastic; Nylon (Polyamide PA); Nylon 66 (PA66); Nylon 66 Fiber

Material Notes: Sanstat CN125 nylon 6,6 monofilaments have electrically conductive carbon suffused into the surface. The filaments have a carbon coating thickness of approximately 1 micron.

Information provided by Shakespeare Company.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.17 g/ccCalculated from diameter of 0.89 mm and product yield of 1374 m/kg.
Fiber Count 6540 denierPer Filament
 
Mechanical PropertiesOriginal ValueComments
Elongation at Break 27 %
Tenacity 3.00 g/denier22.7 kg breaking load
 
Electrical PropertiesOriginal ValueComments
Electrical Resistivity 2000 ohm-cmAverage
 <= 5000 ohm-cm
 
Thermal PropertiesOriginal ValueComments
Melting Point 254 °C
Shrinkage 7.0 %
@Temperature 175 °C,
Time 601 sec

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Shakespeare S-3 Economy Nylon Copolymer Fishing Line, 200 lb
Shakespeare Resistat® F901 N022 Nylon 6 Monofilament
Shakespeare Isocor™ CF140ZI Nylon 6/66

PSHAKE014 / 67293

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.