MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

Trinseo Magnum™ 9015 ABS, High Gloss  (discontinued **)
Categories: Polymer; Thermoplastic; ABS Polymer; Acrylonitrile Butadiene Styrene (ABS), Molded

Material Notes: MAGNUM® ABS resins are thermoplastic materials which provide an excellent balance of processability, impact resistance and heat resistance as imparted by the various polymer compositions. MAGNUM ABS resin are available in a wide range of melt flow rates, impact strength and heat resistance for both high and low gloss applications manufactured by injection molding, sheet or profile extrusion and thermoforming.

The MAGNUM 9000 series of high gloss ABS resins are designed to offer a wide range of impact strengths and melt flow rates to meet the needs of the durables injection molding markets. The 9000 series products offer typical Izod impact strength values from 210 to 400 J/m and melt flow rates ranging from 2.5 to 7.0 g/10min. The gloss values are typically greater than 95% on the 60. Gardner scale for the highest gloss resins and greater than 90% for those products having a broader range of gloss.

MAGNUM® 9015 ABS resin is a high flow, high gloss grade for complex molded parts with thin walls or long flow lengths offering reduced viscosity without sacrificing the toughness, heat resistance or chemical resistance you expect from an ABS resin.

Data provided by Dow Chemical.

This product line was spun off from Dow Chemical to Styron in 2010.

Key Words: Poly(Acrylonitrile Butadiene Styrene)
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.04 g/cc0.0376 lb/in³ASTM Data
Linear Mold Shrinkage 0.0055 cm/cm0.0055 in/in
Melt Flow 12 g/10 min
@Load 3.80 kg,
Temperature 230 °C
12 g/10 min
@Load 8.38 lb,
Temperature 446 °F
ASTM Data
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength, Ultimate 35.2 MPa5110 psiASTM Data
Tensile Strength, Yield 43.4 MPa6290 psiASTM Data
Elongation at Break 45 %45 %ASTM Data
Tensile Modulus 2.41 GPa350 ksiASTM Data
Izod Impact, Notched 2.14 J/cm4.01 ft-lb/inASTM Data
Instrumented Impact Total Energy 22.6 J
@Temperature 23.0 °C
16.7 ft-lb
@Temperature 73.4 °F
 
Thermal PropertiesMetricEnglishComments
Deflection Temperature at 0.46 MPa (66 psi) 93.3 °C200 °FUnannealed; ASTM Data
Deflection Temperature at 1.8 MPa (264 psi) 79.4 °C175 °FUnannealed; ASTM Data
Vicat Softening Point 110 °C230 °F
Flammability, UL94 HB
@Thickness 1.60 mm
HB
@Thickness 0.0630 in
 
Optical PropertiesMetricEnglishComments
Gloss 96 %96 %Gardner Gloss, 60°

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Trinseo Magnum™ 1040 ABS, Very High impact
Trinseo Magnum™ 275 ABS, Low Gloss
Trinseo Magnum™ 2645 ABS, Impact Grade
Trinseo Magnum™ 2642 ABS, Impact Grade
Trinseo Magnum™ 2630 ABS, High Impact

PZZDW101 / 34332

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.