MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

solder replacement adhesives

(Viewing data as-entered. Click here to return)
Lucas-Milhaupt LM 69-241 Silver Braze Alloy
Categories: Metal; Nonferrous Metal; Solder/Braze Alloy

Material Notes: LM 69-241 can be used on any of the common metallic and non-metallic substrates. This alloy will wet ceramics, PCD, CBN, titanium, titanium base and super alloys. LM 69-241 exhibits good wetting characteristics on ceramic surfaces eliminating the metallization and plating processes. Typical applications include brazing of vacuum tubes, wave guides in electrical and electronic industry and PCD, CBN tungsten backed substrates in industrial tool applications. LM 69-241 is generally used in a high vacuum environment. An Argon atmosphere with a dew point of -50°F or better could also be utilized.

Information provided by Lucas-Milhaupt.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 9.29 g/cc
Density 0.336 lb/in³
 
Thermal PropertiesOriginal ValueComments
Melting Point 1148 - 1328 °F
Solidus 1148 °F
Liquidus 1328 °F
 
Processing PropertiesOriginal ValueComments
Processing Temperature 1328 - 1580 °FBrazing Range
 
Component Elements PropertiesOriginal ValueComments
Copper, Cu 23 - 25 %
Indium, In 13 - 15 %
Other, total <= 0.15 %
Silver, Ag 59 - 61 %
Titanium, Ti 2.0 - 2.5 %
 
Descriptive Properties
ColorGray

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

NLUCM9856 / 254797

Solder Replacement
RoHS Compliant Adhesives for Solder Replacement
Master Bond offers RoHS compliant, electrically conductive systems to replace lead soldering. These epoxy and silicone adhesives offer low volume resistivity, low outgassing and high temperature resistance.

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.