Water quenched 845°C (1550°F), 480°C (900°F) temper, 100 mm round. Post water quenched hardness 47 HRC surface, 25 HRC half-radius, 22 HRC center |
ASTM A505, ASTM A519, MIL-SPEC MIL-S-16974, SAE J404, SAE J412, SAE J770, DIN 1.6545, UNI 30 NiCrMo 2 KB, UNS G86300, AMS 6280, AMS 6281, AMS 6530, AMS 6550, ASTM A322, ASTM A331 |