Pro-fax EP495K nucleated, very high impact polypropylene copolymer is available in pellet form. This resin is typically used in extrusion or injection molding applications and offers excellent low temperature impact resistance. Applications: Crates, Pallets/Trays/Tote BinsInformation provided by LyondellBasell. |