MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Versalis KOBLEND HI PD 19 PBT+PC, Impact Grade  (discontinued **)
Categories: Polymer; Thermoplastic; Polycarbonate (PC); Polycarbonate/Polybutylene Terephthalate (PBT) Blend, Unreinforced; Polyester, TP; Polybutylene Terephthalate (PBT)

Material Notes: Symbol according to ISO 1043/1: PBT+PC-HI

Elastomer modified PBT+PC blend with a very good impact behaviour, good stiffness and higher thermal properties than KOBLEND HI 18.

Main application fields: bumpers

Unfilled. Suitable for Injection Molding. Supplied as pellets.

ISO data. Information provided by Enichem

Versalis is the Eni subsidiary containing the plastics and rubber businesses.

Key Words: Polybutylene Terephthalate Polyester + Polycarbonate
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.18 g/cc
Melt Flow 2.2 g/10 min
@Load 2.16 kg,
Temperature 250 °C
cm³/10 min
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength, Yield 43.0 MPa50 mm/min
Elongation at Break >= 50 %Nominal
Elongation at Yield 4.3 %50 mm/min
Tensile Modulus 1.95 GPa1 mm/min
Izod Impact, Unnotched NB
 NB
@Temperature -30.0 °C
Izod Impact, Notched (ISO) 45.0 kJ/m²
@Temperature -30.0 °C
 
Electrical PropertiesOriginal ValueComments
Comparative Tracking Index 500 V
 
Thermal PropertiesOriginal ValueComments
Vicat Softening Point 119 °C50°C/hr; 50N
Flammability, UL94 HB
@Thickness 1.60 mm

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Versalis KOBLEND HI 10 PBT+PC, Impact Grade
Techmer ES Statiblend® ABS GF20 AS 20% Glass Filled
Techmer ES HiFill® ABS GF20 LE 20% Glass Filled
Techmer ES HiFill® ABS GF20 IM 20% Glass Filled
Techmer ES HiFill® ABS GF20 20% Glass Filled

PENJ09 / 35898

Master Bond adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.