MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Specialty Compounds RTP Company

Reynolds Econ® 60 Urethane Rubber
Categories: Polymer; Thermoset; Polyurethane, TS; Thermoset Polyurethane, Elastomer, Unreinforced

Material Notes: Product Overview: Econ™ 60 is an economical and fast curing Shore 60A urethane rubber. It has no odor, features a convenient 1A:1B by volume mix ratio and a low viscosity for easy mixing and pouring. Working time is about 6 minutes and handling time is 4 hours at room temperature. Translucent clear amber color (light passes through) makes Econ™ 60 easy to color with SO Strong™, UVO™ or IGNITE™ colorants. Econ™ 60 is used to make limited run production rubber molds, stamping pads, rubber prototype parts, rubber props and pour-in-place gaskets for industrial equipment. It is also suitable for coating fabrics.

Information provided by Reynolds Advanced Materials

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 1.04 g/cc1.04 g/ccASTM D-1475
Linear Mold Shrinkage <= 0.0010 cm/cm<= 0.0010 in/in
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore A 6060ASTM D-2240
Tensile Strength 2.41 MPa350 psiASTM D-412
Elongation at Break 500 %500 %ASTM D-412
100% Modulus 0.565 MPa82.0 psiASTM D-412
Tear Strength 14.9 kN/m85.0 pliDie C; ASTM D-624
 
Processing PropertiesMetricEnglishComments
Cure Time 240 min4.00 hourHandling Time
 960 min16.0 hour
Pot Life 6.00 min6.00 minASTM D-2471
 
Descriptive Properties
ColorTranslucent Amber
Mix Ratio1A:1Bby volume
 1A:1Bby weight
Specific Volume26.7[cu. in./lb.]

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PREYN089 / 296790

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.