  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

E-Polymers SEPAZ® C140GM 40% Glass Fiber/Mineral Reinforced LCP Resin
Categories: Polymer; Thermoplastic; Liquid Crystal Polymer (LCP)

Material Notes: Liquid Crystal Polymer Resin: SEPAZ LCP resin has a unique structure and performance unthought of in a traditional plastics. Beside SEPAZ LCP takes the excels in all-around performance and molding productivity. SEPAZ LCP has a unique attribute in that the thinner the product becomes, the greater the mechanical strength. SEPAZ LCP finds uses in connectors, sensors and other electronic components and CD pick-up parts, and in copying machine and fax components in office and audio-visual equipment.

Information Provided by E-Polymers Co., Ltd.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 1.73 g/cc1.73 g/ccASTM D792
Water Absorption 0.020 %
@Time 86400 sec
0.020 %
@Time 24.0 hour
Linear Mold Shrinkage 0.0010 cm/cm0.0010 in/in
Linear Mold Shrinkage, Transverse 0.0040 cm/cm0.0040 in/in
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength 111.8 MPa16220 psiASTM D638
Elongation at Break 1.5 %1.5 %ASTM D638
Flexural Strength 163.83 MPa23762 psiASTM D790
Flexural Modulus 13.2 GPa1910 ksiASTM D790
Izod Impact, Notched 0.0686 J/cm0.129 ft-lb/inASTM D256
 
Electrical PropertiesMetricEnglishComments
Volume Resistivity >= 1.00e+14 ohm-cm>= 1.00e+14 ohm-cmASTM D257
Surface Resistance >= 1.00e+15 ohm>= 1.00e+15 ohmASTM D257
Dielectric Constant 3.6
@Frequency 1e+6 Hz
3.6
@Frequency 1e+6 Hz
ASTM D150
Dissipation Factor 0.023
@Frequency 1e+6 Hz
0.023
@Frequency 1e+6 Hz
ASTM D150
 
Thermal PropertiesMetricEnglishComments
Melting Point 335 °C635 °FASTM D789
Deflection Temperature at 1.8 MPa (264 psi) 269 °C516 °FASTM D648
Flammability, UL94 V-0V-0
 
Processing PropertiesMetricEnglishComments
Melt Temperature 350 - 360 °C662 - 680 °F
Mold Temperature 40.0 - 150 °C104 - 302 °F

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Celanese Vectra® A540 Liquid Crystal Polymer (LCP), 40% Mineral Filled
RTP Company RTP 3407-4  Liquid Crystal Polymer (LCP) Glass Fiber 40% - UL94 V-0
Overview of materials for Liquid Crystal Polymer (LCP), Carbon Fiber Filled
Overview of materials for Liquid Crystal Polymer (LCP), 50% Glass Fiber Filled
E-Polymers SEPAZ® C140GP 40% Glass Fiber Reinforced LCP Resin

PEPOLZ064 / 103561

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.