MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
LyondellBasell Microthene® MP675662 Linear Low Density Polyethylene  (discontinued **)
Categories: Polymer; Thermoplastic; Polyethylene (PE); Linear Low Density (LLDPE); Linear Low Density Polyethylene (LLDPE), Rotational Molding Grade

Material Notes: Applications: MICROTHENE MP675662, a hexene LLDPE rotational molding powder with excellent flow properties, can be used to produce a variety of objects such as toys, playground equipment, drums and agricultural and chemical storage containers. MP675662 exhibits good low temperature impact strength and warp resistance. MP675662 is a UV-stabilized, 35-mesh powder and is also available in pellet form as PETROTHENE® GA675662.

Regulatory Status:MP675662 meets the requirements of Food and Drug Administration regulation, 21 CFR 177.1520. This regulation allows the use of this olefin polymer in "...articles or components of articles intended for use in contact with food." Specific limitations or conditions of use may apply.

Information provided by manufacturer.

This product is from the former Equistar product line.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 0.939 g/ccCompression Molded; ASTM D1505
Melt Flow 5.2 g/10 min
@Load 2.16 kg,
Temperature 190 °C
ASTM D1238
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength, Yield 2970 psiCrosshead Speed - 2 in/min; Type IV Specimen (1/8 in); ASTM D638
Flexural Modulus, 1% Secant 126000 psi1/8 in rotomolded sample; ASTM D790
Impact Test 47.0 ft-lbat -40°F; 1/8 in rotomolded sample; ARM STD
 180 ft-lbat -40°F; 1/4 in rotomolded sample; ARM STD
 
Compliance PropertiesOriginal ValueComments
FDA YesSee notes for details.

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
LyondellBasell Microthene® G MU76000 Ethylene Vinyl Acetate Copolymer
LyondellBasell Microthene® G MN72700 Low Density Polyethylene
LyondellBasell Microthene® F FE53200 Ethylene Vinyl Acetate Copolymer
LyondellBasell Microthene MP625962 Linear Low Density Polyethylene (LLDPE)/Hexene, Molded
LyondellBasell Microthene® G MU76300 Ethylene Vinyl Acetate Copolymer

PEQU0760 / 37229

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.