Sequel 1823-UV 7C45 is a mineral filled thermoplastic elastomeric olefin (TEO) resin typically used for exterior molded in color automotive applications. This material exhibits excellent balance of properties and processability. Applications: Automotive Parts, Bumpers, Exterior Automotive ApplicationsInformation provided by LyondellBasell. |