MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

(Viewing data as-entered. Click here to return)
Lanxess Aflux® 16 Processing Aid
Categories: Other Engineering Material; Additive/Filler for Polymer

Material Notes: Function: Processing promoter for polymeric compounds, mainly based on EPDM and IIR

Use: Aflux 16 improves the flow properties of polymeric compounds by reducing viscosity and promoting slippage at the rubber-to-metal interface. This leads to higher extrusion rates, improved dimensional stability and a constant level of die swell. During injection molding Aflux 16 improves mold flow. It prevents sticking to the metal surfaces and enhances demolding without mold fouling. It is recommended to use Aflux 16 when the mold has a complicated geometry. At the mixing stage Aflux 16 prevents sticking to roll surfaces and the rotors of the internal mixer. Aflux 16 has an activating effect on the cross-linking rate of sulfur cross- linked polymer compounds. In CR compounds Aflux 16 has a stabilizing effect. Processing safety is increased.

Application: Polymer compounds, primarily based on EPDM and IIR. Reduces the viscosity of rubber mixes. Reduces sticking to mixing units, aids removal of vulcanizates from the mold.

Information provided by Lanxess.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.03 g/cc
Ash 6.4 %
 
Chemical PropertiesOriginal ValueComments
Acid Value <= 22[mg KOH/g]
 
Thermal PropertiesOriginal ValueComments
Melting Point 80.0 - 105 °C
 
Processing PropertiesOriginal ValueComments
Shelf Life 36.0 Month
 
Descriptive Properties
Appearancebeige Pellets

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Lanxess Uniplex 260 Plastic Additive
3M Dyneon™ Dynamar™ FX 5920B Polymer Processing Additive

PLANY8238 / 208631

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.