MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Specialty Compounds RTP Company

Total 9460 HDPE Film Grade
Categories: Polymer; Film; Thermoplastic; Polyethylene (PE); High Density (HDPE); High Density Polyethylene (HDPE), Film Grade

Material Notes: High Barrier grade, good processability, high stiffness, low gels

Applications: Cereal liners, cracker over-wrap, bakery mixes, specialty monolayer films, coextruded films

Information provided provided by Total Petrochemicals.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 0.962 g/cc0.0348 lb/in³ASTM D792
Water Vapor Transmission 1.90 g/m²/day
@Thickness 0.0508 mm
0.122 g/100 in²/day
@Thickness 0.00200 in
100°F; ASTM F1249
Thickness 25.4 microns1.00 milas tested; 2.5 BUR
Melt Flow 2.0 g/10 min
@Load 2.16 kg,
Temperature 190 °C
2.0 g/10 min
@Load 4.76 lb,
Temperature 374 °F
ASTM D1238
 
Mechanical PropertiesMetricEnglishComments
Film Tensile Strength at Yield, MD 29.0 MPa
@Thickness 0.0508 mm
4200 psi
@Thickness 0.00200 in
ASTM D882A
Film Tensile Strength at Yield, TD 24.8 MPa
@Thickness 0.0508 mm
3600 psi
@Thickness 0.00200 in
ASTM D882A
Film Elongation at Break, MD 850 %
@Thickness 0.0508 mm
850 %
@Thickness 0.00200 in
ASTM D882A
Film Elongation at Break, TD 500 %
@Thickness 0.0508 mm
500 %
@Thickness 0.00200 in
ASTM D882A
1% Secant Modulus, MD 965 MPa
@Thickness 0.0508 mm
140000 psi
@Thickness 0.00200 in
ASTM D882A
1% Secant Modulus, TD 1240 MPa
@Thickness 0.0508 mm
180000 psi
@Thickness 0.00200 in
ASTM D882A
 
Processing PropertiesMetricEnglishComments
Melt Temperature 193 - 216 °C380 - 420 °F
 
Descriptive Properties
ProcessFilm

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PTOTAL698c / 221023

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.