MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Teknor Apex Telcar® TL-1654D Thermoplastic Elastomer
Categories: Polymer; Thermoplastic; Elastomer, TPE; Vinyl (PVC); PVC, Wire and Cable Grade

Material Notes: Notes: Non-halogenated; RoHS Compliant; MBDC: Green

Uses: Automotive Applications; Automotive Exterior Parts; Automotive Exterior Trim; Automotive Interior Parts; Blow Molding Applications; General Purpose; Grommets; Weatherstripping; Wire and Cable Applications

Forms: Pellets

Processing Method: Extrusion; Injection Molding

Injection Notes: Injection Rate: Moderate-Fast

Extrusion Notes: Screw Speed: 30 to 100 rpm

Information Provided by Teknor Apex

Key Words: TPE
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 1.29 g/ccASTM D792
Melt Flow 1.0 g/10 min
@Load 2.16 kg,
Temperature 190 °C
ASTM D1238
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore D 53ASTM D2240
Tensile Strength at Break 1200 psiASTM D412
Elongation at Break 530 %ASTM D412
 
Electrical PropertiesOriginal ValueComments
Dielectric Constant 2.9
@Frequency 1e+6 Hz
ASTM D150
 3.0
@Frequency 1000 Hz
ASTM D150
Dielectric Strength 800 V/milASTM D419
 
Thermal PropertiesOriginal ValueComments
Brittleness Temperature -56.2 °FASTM D746
Oxygen Index 24 %ASTM D2863
 
Processing PropertiesOriginal ValueComments
Rear Barrel Temperature 340 - 380 °F
Middle Barrel Temperature 350 - 390 °F
Front Barrel Temperature 360 - 400 °F
Nozzle Temperature 370 - 410 °F
Zone 1 330 - 370 °F
Zone 2 340 - 380 °F
Zone 3 350 - 390 °F
Zone 5 360 - 400 °F
Die Temperature 374 - 410 °F
Melt Temperature 370 - 410 °FProcessing Temperature
Mold Temperature 77.0 - 150 °F
Injection Pressure 200 - 1000 psi
Back Pressure 25.0 - 50.0 psi
Cushion 0.150 - 1.00 in
Screw Speed 50 - 100 rpm
 
Descriptive Properties
AppearanceOpaque

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Teknor Apex Sinvicomp SBC 3707 Polyvinyl Chloride, Rigid
Teknor Apex Sinvicomp SBB 3713 Polyvinyl Chloride, Rigid
Teknor Apex Sinvicomp SBB 3710 Polyvinyl Chloride, Rigid
Teknor Apex Sinvicomp SBB 3700 Polyvinyl Chloride, Rigid
Celanese Hytrel® RS R4275 BK316 Polyester Elastomer TPC-ET

PTEKNP412 / 129493

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.