MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

DuPont Mobility and Materials Delrin® 100PE BK602 POM  (discontinued **)
Categories: Polymer; Thermoplastic; Acetal (Polyoxymethylene, POM)

Material Notes: High Viscosity Acetal Homopolymer with Very Low Emissions

Information provided by DuPont; The Delrin product line was sold by DuPont in 2023 but this specific grade was discontinued prior to the sale

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.42 g/cc0.0513 lb/in³ISO 1183
Melt Density 1.19 g/cc
@Temperature >=178 °C
0.0430 lb/in³
@Temperature >=352 °F
Water Absorption 0.94 %
@Thickness 2.00 mm
0.94 %
@Thickness 0.0787 in
Sim. to ISO 62
Moisture Absorption 0.200 %
@Thickness 2.00 mm
0.200 %
@Thickness 0.0787 in
Sim. to ISO 62
Linear Mold Shrinkage, Flow 0.022 cm/cm0.022 in/inISO 294-4, 2577
Linear Mold Shrinkage, Transverse 0.018 cm/cm0.018 in/inISO 294-4, 2577
Melt Flow  1.8 g/10 min
@Load 2.16 kg,
Temperature 190 °C
1.8 g/10 min
@Load 4.76 lb,
Temperature 374 °F
from MVR and melt density; ISO 1133
 2.5 g/10 min
@Load 2.16 kg,
Temperature 190 °C
2.5 g/10 min
@Load 4.76 lb,
Temperature 374 °F
ISO 1133
 
Mechanical PropertiesMetricEnglishComments
Hardness, Rockwell M 9292ISO 2039-2
Hardness, Rockwell R 120120ISO 2039-2
Tensile Strength, Yield 72.0 MPa10400 psiISO 527-1/-2
Elongation at Break 38 %38 %ISO 527-1/-2
Elongation at Yield 21 %21 %ISO 527-1/-2
Tensile Modulus 3.10 GPa450 ksiISO 527-1/-2
Flexural Yield Strength 80.0 MPa
@Strain 3.5 %
11600 psi
@Strain 3.5 %
ISO 178
Flexural Modulus 2.90 GPa421 ksiISO 178
Poissons Ratio 0.370.37ISO 527-1/-2
Charpy Impact Unnotched  30.0 J/cm²
@Temperature -30.0 °C
143 ft-lb/in²
@Temperature -22.0 °F
ISO 179/1eU
 35.0 J/cm²
@Temperature 23.0 °C
167 ft-lb/in²
@Temperature 73.4 °F
ISO 179/1eU
Charpy Impact, Notched  1.00 J/cm²
@Temperature -30.0 °C
4.76 ft-lb/in²
@Temperature -22.0 °F
ISO 179/1eA
 1.10 J/cm²
@Temperature 23.0 °C
5.23 ft-lb/in²
@Temperature 73.4 °F
ISO 179/1eA
 
Electrical PropertiesMetricEnglishComments
Volume Resistivity >= 1.00e+15 ohm-cm>= 1.00e+15 ohm-cmIEC 62631-3-1
Surface Resistance 5.00e+13 ohm5.00e+13 ohmIEC 62631-3-2
Dielectric Constant  3.9
@Frequency 1e+6 Hz
3.9
@Frequency 1e+6 Hz
IEC 62631-2-1
 3.9
@Frequency 100 Hz
3.9
@Frequency 100 Hz
IEC 62631-2-1
Dielectric Strength 44.0 kV/mm1120 kV/inIEC 60243-1
Dissipation Factor  0.00050
@Frequency 100 Hz
0.00050
@Frequency 100 Hz
IEC 62631-2-1
 0.0055
@Frequency 1e+6 Hz
0.0055
@Frequency 1e+6 Hz
IEC 62631-2-1
Comparative Tracking Index 600 V600 VIEC 60112
 
Thermal PropertiesMetricEnglishComments
CTE, linear, Parallel to Flow 110 µm/m-°C61.1 µin/in-°FISO 11359-1/-2
 100 µm/m-°C
@Temperature -40.0 - 23.0 °C
55.6 µin/in-°F
@Temperature -40.0 - 73.4 °F
ISO 11359-1/-2
CTE, linear, Transverse to Flow 110 µm/m-°C61.1 µin/in-°FISO 11359-1/-2
 100 µm/m-°C
@Temperature -40.0 - 23.0 °C
55.6 µin/in-°F
@Temperature -40.0 - 73.4 °F
ISO 11359-1/-2
Melting Point 178 °C352 °F10°C/min; ISO 11357-1/-3
Deflection Temperature at 0.46 MPa (66 psi) 158 °C316 °FISO 75-1/-2
Deflection Temperature at 1.8 MPa (264 psi) 97.0 °C207 °FISO 75-1/-2
Flame Spread 28.0 mm/min
@Thickness 1.00 mm
1.10 in/min
@Thickness 0.0394 in
DS; ISO 3795 (FMVSS 302)
 
Processing PropertiesMetricEnglishComments
Melt Temperature 195 - 205 °C383 - 401 °FExtrusion
 200 °C392 °FExtrusion Optimum
 205 °C401 °FInjection Optimum
 200 - 210 °C392 - 410 °FInjection
Mold Temperature 80.0 - 100 °C176 - 212 °FInjection
 90.0 °C194 °FInjection Optimum
Drying Temperature 75.0 °C167 °FExtrusion
 80.0 °C176 °FInjection
 85.0 °C185 °FExtrusion
Dry Time 2.00 - 4.00 hour2.00 - 4.00 hourDehumidified Dryer; Extrusion
 2.00 - 4.00 hour2.00 - 4.00 hourDehumidified Dryer; Injection
Moisture Content 0.20 %0.20 %Extrusion
 0.20 %0.20 %Injection
Hold Pressure 90.0 - 110 MPa13100 - 16000 psiInjection
Annealing Temperature 160 °C320 °FInjection
 
Descriptive Properties
AdditivesRelease agent
Annealing time30 min/mmInjection - Optional
Delivery formPellets
Drying RecommendedyesInjection
Emissions<2 mg/kgVDA 275
FMVSS ClassBISO 3795 (FMVSS 302)
Hold pressure time (s/mm)8Injection
Part Marking CodePOMISO 11469
ProcessingInjection Molding
 Other Extrusion
 Profile Extrusion
 Sheet Extrusion
Regional AvailabilityAsia Pacific
 Europe
 Global
 Near East/Africa
 North America
 South and Central America
Resin IdentificationPOMISO 1043

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Delrin Delrin® 100P BK602 POM
Delrin Delrin® 100 BK602 POM
Delrin Delrin® 100P NC010 POM
Delrin Delrin® 150 NC010 POM
DuPont Mobility and Materials Delrin® II150E BK602 Acetal (POM)

PDSX5087 / 197727

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.