MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Specialty Compounds RTP Company

Multibase Multi-Flex® A 8832 TPE Thermoplastic Elastomer
Categories: Polymer; Thermoplastic; Elastomer, TPE

Material Notes:

Features:

  • Chemical Resistance, Good
  • Thermal Stability, Good
  • Ozone Resistant
  • Noise Damping
  • Forms:

  • Pellets
  • Processing Method:

  • Injection Molding
  • Uses:

  • Automotive Applications
  • Information provided by Multibase

    Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
     
    Physical PropertiesMetricEnglishComments
    Specific Gravity 1.92 g/cc1.92 g/ccASTM 792
    Linear Mold Shrinkage 0.012 cm/cm0.012 in/inASTM D955
    Melt Flow 12 g/10 min
    @Load 2.16 kg,
    Temperature 230 °C
    12 g/10 min
    @Load 4.76 lb,
    Temperature 446 °F
    ASTM D1238
     
    Mechanical PropertiesMetricEnglishComments
    Hardness, Shore A 939310 seconds; ASTM D2240
    Tensile Strength, Yield 5.52 MPa800 psiElastic; ASTM D638
    Elongation at Break 320 %320 %ASTM D638
    Flexural Modulus 0.310 GPa45.0 ksiASTM D790
    Tear Strength 35.1 kN/m200 pliASTM D624

    Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

    Users viewing this material also viewed the following:
    Covestro Desmopan® 487 Thermoplastic Polyurethane
    BASF Elastollan® C 85 A HPM TPUR
    712BNF Cork/Nitrile Rubber Sheet
    SK Chemicals SKYTHANE® S185A Polyester Based Thermoplastic Polyurethane Elastomer
    Northstar Polymers MGB-A90A High Performance Polyurethane Cast Elastomer System 90A

    PMULTI063 / 53967

    Free Trade Publications, Click Here!
    Free Trade Publications, Click Here!

    Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

    The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.