MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Specialty Compounds RTP Company

EOS Titanium Ti64 Grade 5 DMSL on EOS M 400-4; 80 µm Layer Thickness
Categories: Metal; 3D Printing/Additive Manufacturing Metal; Nonferrous Metal; Titanium Alloy

Material Notes: EOS Titanium Ti64 Grade 5 is a Ti6Al4V alloy, which is well-known for having excellent mechanical properties: low density with high strength and excellent corrosion resistance. The alloy has low weight compared to superalloys and steels and higher fatigue resistance compared to other lightweight alloys. Parts built with EOS Titanium Ti64 Grade 5 powder can be machined, shot-peened and polished in as manufactured and heat treated states. Due to the layerwise building method, the parts have a certain anisotropy. Heat treatment is recommended to reduce internal stresses and increase ductility. EOS Titanium Ti64 Grade 5 powder can be used on the EOS M 290 with a 40 µm and 80 µm process and on the EOS M 400-4 with an 80 µm process.

Main Characteristics:

  • Low weight combined with high strength
  • Excellent corrosion resistance
  • High fatigue resistance compared to other lightweight alloys
  • The parts fulfill chemical requirements for Grade 5 alloy
Typical Applications:
  • Aerospace components
  • Automotive components
  • Other industrial applications where low weight in combination with high strength are required

Information provided by EOS GmbH (Electro Optical Systems).

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Particle Size 20 - 80 µm20 - 80 µm
Thickness 80.0 microns3.15 mil
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength 1000 MPa145000 psiHIP horizontal
 1010 MPa146000 psiHIP vertical
 1090 MPa158000 psiHeat treated horizontal
 1090 MPa158000 psiHeat treated vertical
Tensile Strength, Yield 890 MPa129000 psiHIP horizontal
 910 MPa132000 psiHIP vertical
 990 MPa144000 psiHeat treated horizontal
 1010 MPa146000 psiHeat treated vertical
Elongation at Break 14 %14 %Heat treated vertical
 15 %15 %Heat treated horizontal
 16 %16 %HIP horizontal
 16 %16 %HIP vertical
Reduction of Area >= 25 %>= 25 %Heat treated horizontal
 >= 25 %>= 25 %Heat treated vertical
 >= 25 %>= 25 %HIP horizontal
 >= 25 %>= 25 %HIP vertical
Fatigue Strength 563 MPa
@# of Cycles 1.00e+7
81700 psi
@# of Cycles 1.00e+7
ASTM E466
 
Component Elements PropertiesMetricEnglishComments
Aluminum, Al 5.5 - 6.75 %5.5 - 6.75 %
Carbon, C <= 0.080 %<= 0.080 %
Hydrogen, H <= 0.015 %<= 0.015 %
Iron, Fe <= 0.30 %<= 0.30 %
Nitrogen, N <= 0.050 %<= 0.050 %
Other, each <= 0.10 %<= 0.10 %
Other, total <= 0.40 %<= 0.40 %
Oxygen, O <= 0.20 %<= 0.20 %
Titanium, Ti 87.6 - 91 %87.6 - 91 %Balance
Vanadium, V 3.5 - 4.5 %3.5 - 4.5 %
Yttrium, Y <= 0.0050 %<= 0.0050 %
 
Descriptive Properties
Surface roughness9 µmRa, Vertical
Volume rate4 x 12.0 mm³/s

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

NEOS961 / 280621

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.