MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

Lanxess Addonyl® 8073 Nylon Casting Aid
Categories: Other Engineering Material; Additive/Filler for Polymer

Material Notes: Cast Nylon 6, a plastic of high molecular weight, is produced through an anionic polymerization of caprolactam. During the pressureless casting process the monomeric caprolactam melt is poured into the mold and directly polymerized by a specific chemical reaction and then forms a semi-finished product or molding. Addonyl® 8073 is used in combination with the catalyst Addonyl® Kat NL and the activator Addonyl® 8120 during the production of Cast Nylon (PA-6 G). This allows users to combine various properties, and to tailor materials specifically to requirements.

Addonyl® 8073 is a solid high-molecular-weight polyol. Addonyl® 8073 is used in rotomolding to prevent the formation of voids and pinholes. It also improves the impact value and the machinability of the obtained cast nylon. Addonyl® 8073 has the following advantages:

  • Colorless, wax-like flakes
  • The product is easily soluble in molten caprolactam without residue
Use: The reactivity of the polymerizing melt is influenced by various factors. Lanxess advises against a concentration of > 2% p.b.w., because problems with the polymerization may occur.

Information provided by Lanxess.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Water Absorption <= 0.50 %<= 0.50 %
 
Thermal PropertiesMetricEnglishComments
Melting Point 60.0 °C140 °F
 
Processing PropertiesMetricEnglishComments
Melt Temperature 110 - 130 °C230 - 266 °F
Mold Temperature 130 - 160 °C266 - 320 °F
Shelf Life 12.0 Month12.0 Month
 
Descriptive Properties
Appearancecolorless, waxy flakes
Hydroxyl value<7 mg KOH/g

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PLANY8216 / 208609

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.