MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

(Viewing data as-entered. Click here to return)
Domo TechnylStar™ S 218 V35 PA6, 35% glass filled
Categories: Polymer; Thermoplastic; Nylon (Polyamide PA); Nylon 6 (PA6); Nylon 6, 40% Glass Fiber Filled

Material Notes: TECHNYLSTAR Polyamide, reinforced with 35% of glass fiber, heat stabilized, for injection molding. Characterized by a high fluidity of the melt.

Available in: Europe and North America

Product Applications: Due to its outstanding flow characteristics, TECHNYL STAR S 218 V35 BLACK 31N provides a significant productivity improvement and allows more freedom in mould design and part design versus standard polyamide solutions. This product is available in black.

Product data for dry samples.

DOMO Chemicals has acquired Solvay’s Performance Polyamides Business in Europe.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.41 g/ccISO 1183/A
Water Absorption 0.90 %
@Temperature 23.0 °C,
Time 86400 sec
ISO 62
Linear Mold Shrinkage 0.0042 cm/cmIsotropy
Linear Mold Shrinkage, Flow 0.0030 cm/cm
Linear Mold Shrinkage, Transverse 0.0053 cm/cm
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength at Break 195 MPaISO 527 Type 1A
Elongation at Break 3.0 %ISO 527 Type 1A
Tensile Modulus 10700 MPaISO 527 Type 1A
Flexural Strength 295 MPaISO 178
Flexural Modulus 10000 MPaISO 178
Izod Impact, Notched (ISO) 13.0 kJ/m²ISO 180/1eA
Izod Impact, Unnotched (ISO) 75.0 kJ/m²ISO 180/1eU
Charpy Impact Unnotched 75.0 kJ/m²ISO 179/1eU
Charpy Impact, Notched 13.0 kJ/m²ISO 179/1eA
 
Thermal PropertiesOriginal ValueComments
Melting Point 222 °CISO 11357
Deflection Temperature at 1.8 MPa (264 psi) 210 °CISO 75/Af
Flammability, UL94 HB
@Thickness 1.60 mm
1210
Glow Wire Flammability Index 650 °C
@Thickness 1.60 mm
ISO 60695-2-12
 
Processing PropertiesOriginal ValueComments
Feed Temperature 220 - 225 °C
Mold Temperature 80.0 °C
Drying Temperature 80.0 °C
Moisture Content <= 0.20 %
 
Descriptive Properties
Compression Zone225-235°C
Mixing Zone235-245°C

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Envalior Akulon® K222-KGV4 PA6-GF20 FR(30), Dry, 20% Glass Filled, Heat Stabilized, Flame Retardant
Akro-Plastic Akromid® B3 K8 9 FR grey (3840) PA6 FR, Dry, 20% Glass Filled
Akro-Plastic Akromid® B3 K8 9 FR grey (3840) PA6 FR, Conditioned, 20% Glass Filled
Domo TechnylStar™ S 216 V35 PA6, 35% glass filled, DRY
Domo Technyl® C216V25 25% Glass Filled Nylon 6

PRHOD835 / 138066

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.