MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
LyondellBasell Alathon H 5057 High Denisty Polyethylene  (discontinued **)
Categories: Polymer; Thermoplastic; Polyethylene (PE); High Density (HDPE); High Density Polyethylene (HDPE), Injection Molded

Material Notes: Alathon high density polyethylene resins are produced in North America using slurry and solution technologies and include bi-modal HMW grades commonly used in pressure pipe and blown film, general purpose and thin-wall injection molding grades, and blown film grades known for their moisture barrier performance.

Alathon H5057 is a multi-purpose high-flow resin that exhibits enhanced low temperature impact performance, enhanced processing and thermal stability for fast cycling in multi-cavity stack molds, good color and organoleptic properties. Typical applications are rigid food containers such as cultured dairy product containers, margarine tubs, butter tubs, small frozen food containers and promotional drink cups. Applications: TWIM Food Containers

Information provided by LyondellBasell.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Bulk Density 37.0 - 39.0 lb/ft³ASTM D1895
Density 0.948 g/ccASTM D1505
Melt Flow 57 g/10 min
@Load 2.16 kg,
Temperature 190 °C
ASTM D1238
Spiral Flow 53.8 cmLYB Method
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore D <= 69ASTM D2240
Tensile Strength at Break 19.0 MPaASTM D638
Elongation at Break 4.1 %ASTM D638
Tensile Modulus 683 MPa1% secant; ASTM D638
Flexural Modulus, 1% Secant 972 MPaASTM D790
2% Secant Modulus 820 MPaASTM D790
Izod Impact, Notched 21.0 J/m
@Temperature 23.0 °C
ASTM D256
Izod Impact, Unnotched 330 J/m
@Temperature -18.0 °C
ASTM D4812
 
Thermal PropertiesOriginal ValueComments
Melting Point 126.2 °CASTM D3418
Crystallization Temperature 113.4 °CASTM D3418
Deflection Temperature at 0.46 MPa (66 psi) 64.0 °Cunannealed; ASTM D648
Vicat Softening Point 118 °CASTM D1525
 
Descriptive Properties
Processing MethodInjection Molding

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
LyondellBasell Hostalen 5231H High Density Polyethylene (HDPE), Injection Molded
Chevron Phillips Marlex® 9012C Polyethylene HDPE, Injection Molding Grade
Dow DOWLEX™ IP-10 High Density Polyethylene
LyondellBasell Alathon M 6080UV High Denisty Polyethylene
LyondellBasell Alathon® M6080WC High Density Polyethylene

PEQT7061 / 218699

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.