MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
SCG Chemicals EL-Pro™ P600F Polypropylene Film Resin
Categories: Polymer; Film; Thermoplastic; Polypropylene (PP); Polypropylene, Film Grade

Material Notes: Key Characteristics:
  • Good optical properties
  • High productivity
  • Good openability with 3000 ppm slip agent and 2700 ppm antiblocking agent

Recommended Applications:

  • Water quenched blown film for food and apparel packaging

Information provided by SCG Chemicals

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 0.910 g/ccASTM D1505
Thickness 25.0 microns
Melt Flow 10 g/10 min
@Load 2.16 kg,
Temperature 230 °C
ASTM D1238
 
Mechanical PropertiesOriginal ValueComments
Film Tensile Strength at Yield, MD 28.0 MPaASTM D882
Film Tensile Strength at Yield, TD 20.0 MPaASTM D882
Film Elongation at Break, MD 850 %ASTM D882
Film Elongation at Break, TD 770 %ASTM D882
Flexural Modulus 17000 kg(f)/cm²ASTM D790
Secant Modulus, MD 0.690 GPaASTM D882
Secant Modulus, TD 0.540 GPaASTM D882
Izod Impact, Notched 2.50 kg-cm/cmASTM D256
Film Tensile Strength at Break, MD 27.0 MPaASTM D882
Film Tensile Strength at Break, TD 26.0 MPaASTM D882
 
Thermal PropertiesOriginal ValueComments
Melting Point 160 °CASTM D2117
Deflection Temperature at 0.46 MPa (66 psi) 110 °CASTM D648
Vicat Softening Point 155 °CASTM D1525
Brittleness Temperature <= -10.0 °CASTM D746
 
Optical PropertiesOriginal ValueComments
Haze 9.0 %ASTM D1003
Gloss 55 %ASTM D2457

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
SCG Chemicals EL-Pro™ P401S Polypropylene Flat Yarn/Sheet
SCG Chemicals EL-Pro™ P700J Polypropylene Injection Molding
Lotte Chemical Titan TITANPRO® PD943 Polypropylene homopolymer
Global PP-1126-NK Polypropylene Homopolymer
Global PP-1100-PK Polypropylene Homopolymer

PSCGC950 / 120704

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.