MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

Shinil Chemical SHINNANO PA-66 Polymer Nanocomposite CHC
Categories: Polymer; Thermoplastic; Nylon (Polyamide PA); Nylon 66 (PA66)

Material Notes: SHINNANO is the product line of polymer nanocomposite made by dispersing nano fillers, mainly, NANOCLAY. Shinil has developed various nanocomposite grades for automotive applications using proprietary dispersion technology combined with the customized nanoclay. Nanocomposite products of SHINNANO provide not only high performance but also the lighter weight (10-20%).

SHINNANO uses various engineering polymers to produce functional nanocomposite grades. Nanoclays are incorporated during the melt compounding. The clay particles are exfoliated during processing, which leads to nano-size platelets. Although this process is challenging, owing to unique dispersion technique that is developed for nano materials, Shinil produces high performance nanocomposites with less use of nano fillers. SHINNANO grades are available for automotive parts such as bumper, instrument panel, door trim, engine cover, cylinder head cover, and air intake manifold.

Feature and Benefits

  • Lighter weight
  • High stiffness
  • High HDT
  • High modulus
  • Improved surface
  • Improved melt strength
  • Recyclability
  • Available for injection modling, extrusion or film making
  • Cost effective
  • Good barrier property

Information Provided by Shinil Chemical Industry Co., Ltd.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 1.34 g/cc1.34 g/cc
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength, Ultimate 147 MPa21300 psi
Elongation at Break 3.0 %3.0 %
Flexural Strength 255.06 MPa36993 psi
Flexural Modulus 8.34 GPa1210 ksi
Izod Impact, Notched 0.588 J/cm1.10 ft-lb/in
 
Thermal PropertiesMetricEnglishComments
Deflection Temperature at 1.8 MPa (264 psi) 245 °C473 °F
 
Processing PropertiesMetricEnglishComments
Processing Temperature 260 °C500 °F

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Overview of materials for Silicone Rubber
Taiwan PU Corporation UR60 Polyester Urethane Rubber
Taiwan PU Corporation UR50 Polyester Urethane Rubber
Overview of materials for Liquid Silicone Rubber
ATG s.r.l. EACM Ethylene-Acrylic Rubber

PSHINL24 / 104026

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.