MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

(Viewing data as-entered. Click here to return)
Celanese Celcon® TX86 Ductile Acetal Copolymer
Categories: Polymer; Thermoplastic; Acetal (Polyoxymethylene, POM); Acetal Copolymer, Impact Modified

Material Notes: Description: Celcon TX86 is a slightly toughened acetal copolymer which exhibits ductility in bending and impact loading. The ductile rather than brittle, failure mode gives engineers greater design freedom in applications such as clips, fasteners, gears and rollers.

Information provided by Celanese Corporation.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.40 g/ccISO 1183
Linear Mold Shrinkage 0.017 cm/cmASTM D955
Linear Mold Shrinkage, Transverse 0.015 cm/cmASTM D955
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength, Yield 58.0 MPa50 mm/min; ISO 527-2/1A
Tensile Modulus 2.45 GPa1 mm/min; ISO 527-2/1A
Flexural Modulus 2.16 GPaISO 178
Izod Impact, Notched (ISO) 8.00 kJ/m²ISO 180/1A
 
Thermal PropertiesOriginal ValueComments
Deflection Temperature at 1.8 MPa (264 psi) 88.0 °CISO 75-1, -2
 
Processing PropertiesOriginal ValueComments
Melt Temperature 182 - 199 °C
Mold Temperature 77.0 - 93.0 °C
Drying Temperature 180 °F
Dry Time 3 hour
Injection Pressure 11000 - 16000 psi

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Celanese Celcon® TX90 Acetal Copolymer
Celanese Celcon® EC90PLUS Acetal Copolymer
Celanese Celcon® GB10 POM, 10% Glass Reinforced
Celanese Celcon® EF10 Acetal Copolymer, 10% Carbon Fiber
Celanese Celcon® EC15C Conductive Grade Acetal Copolymer

PHCW11 / 45952

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.