MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Akrochem AKROCHEM® GUM ROSIN
Categories: Wood and Natural Products

Material Notes: Product Description: Akrochem Gum Rosin is a 75°C softening point, low molecular weight rosin gum produced from natural, renewable resources. This rosin’s distinctive feature is that it contains acid functionality (-COOH), making it compatible in a wide range of elastomers. This rosin is appropriate for use in rubber products, sealants, coatings, adhesives and printing inks.

Applications: Gum Rosin is utilized in rubber products as a low-cost tackifier and softener in hoses, belts, footwear, flooring and molded goods, etc. This rosin aids in processing of a wide range of elastomers compounds by increasing green tack, rate of incorporation of fillers, stock flow and improves knitting. Gum Rosin is recommended for light colored stocks and typical loading range is 10 – 25 phr. Gum Rosin is FDA acceptable under CFR 21 section 175.105 (Adhesives) and 177.2600 (Rubber Articles Intended for Repeated Use).

Information provided by Akrochem Corporation

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 1.07 g/cc
 
Chemical PropertiesOriginal ValueComments
Acid Value 150 - 175[mg KOH/g]
 
Thermal PropertiesOriginal ValueComments
Ring & Ball Softening Point 65.0 - 80.0 °C
 
Optical PropertiesOriginal ValueComments
Gardner Color Number <= 7.050% toluene
 
Descriptive Properties
Appearancetransparent solid

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PAKZCH347 / 315265

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.