Desmodur E 15 is an aromatic polyisocyanate prepolymer based on toluene diisocyanate (TDI). It is suitable for use in the formulation of flexible coatings and sealing compounds. Properties / Applications: Desmodur E 15 can be combined with Hardener DT to formulate highly reactive two-component systems which yield highly flexible high build coatings, e. g. for use as crack bridging coatings on concrete surfaces. Combination with latent hardener (bisoxazolidine) produces highly flexible one-component systems, e. g. for coating flat roofs. As with any product, use of Desmodur E 15 in a given application must be tested (including but not limited to field testing) in advance by the user to determine suitability. Information provided by Covestro |