MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Elmet Technologies

(Viewing data as-entered. Click here to return)
SunChemical Gwent C2110817D5 Conductive Silver Polymer Paste
Categories: Metal; Other Engineering Material; Ceramic/Metallic Coating; Polymer; Thermoplastic; Adhesives, Sealants, and Coatings

Material Notes: This product is a thermoplastic screen printing ink, developed for use in membrane touch switch applications as well as counter electrode in electro-chemical sensors and conductive tracks. It may be screen printed on to flexible polymeric substrates, such as Polyimide, PEN and PET substrates, to create a highly conductive track for general circuitry. The ink has under gone electrical and mechanical testing which has shown that it is flexible. The product has excellent adhesion properties (tougher film) with faster evaporating solvents and exhibits good conductivity.
Screen Printing Equipment: semi-automatic, manual
Screen Types: stainless steel, polyester, mesh 156 to 325tpi
Substrate: Polyester, PVC, Polycarbonate, or Ceramic.

Information provided by Gwent Electronic Materials Ltd.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Solids Content 64.5 - 65.5 %
@Temperature 700 °C
Viscosity 22000 - 27000 cP
@Shear Rate 230 1/s,
Temperature 25.0 °C
Haake VT 550 PK1.1°
Thickness 20.0 - 30.0 micronsUsing a 230 stainless steel mesh screen
Storage Temperature 20.0 °Csealed container
 
Electrical PropertiesOriginal ValueComments
Surface Resistivity per Square 0.025 - 0.035 ohm
@Thickness 0.0250 mm
Using a 230 stainless steel mesh screen
 0.070 - 0.077 ohm
@Thickness 0.0100 mm
Using a 230 stainless steel mesh screen
 
Processing PropertiesOriginal ValueComments
Cure Time 5.00 min
@Temperature 170 °C
belt dryer
 10.0 min
@Temperature 130 °C
belt dryer
 10.0 min
@Temperature 150 °C
box oven
 30.0 min
@Temperature 130 °C
box oven
Shelf Life 6.00 Month
 
Descriptive Properties
Coverage cm2/g121.77Using a 230 stainless steel mesh screen

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
SunChemical Gwent R2070613P2 Resin Binder
SunChemical Gwent D2070209P6 White Dielectric Paste
SunChemical Gwent D2020409D8 Dielectric for Stainless Steel
SunChemical Gwent C2110127D3 Nanocopper based Paste
SunChemical Gwent C2100211D1 Silicone Based Silver Paste

WGELZ9034 / 139347

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.